CBC of the. IGZO semiconductor layer on Si/SiO2 substrates was first optimized, yielding the parameters: 10 mm sec-1 coating speed, 100 µm gap height, 70 °C …
CBC of the. IGZO semiconductor layer on Si/SiO2 substrates was first optimized, yielding the parameters: 10 mm sec-1 coating speed, 100 µm gap height, 70 °C …