InGaN nanorods offer a three-dimensional platform for optoelectronic structures, but their geometry also makes composition control more complex than in planar films. A nanoscale study of InGaN/GaN core-shell nanorods has directly imaged indium-rich triangular regions at the edges of the rods. These nanoprisms emit at longer wavelengths than the surrounding InGaN shell, revealing substantial variation in composition across different facets of the same structure.

For engineers and technical decision-makers working with semiconductor materials, the result highlights an important process consideration: a nominal shell thickness does not necessarily mean uniform material properties. Local growth conditions at edges and sidewalls can produce distinct optical and structural domains.

Why composition varies in InGaN nanorods

InGaN/GaN core-shell nanorods combine a GaN core with an InGaN shell. Their three-dimensional shape provides a large active surface area and exposes crystal facets with different orientations. Compared with planar growth, however, depositing a consistent shell around a nanorod presents additional challenges. Understanding how indium enters the InGaN layer is important because composition affects the material’s optical emission.

The nanorods examined in the study were grown by selective-area metal-organic vapor-phase epitaxy. The process formed Si-doped GaN rods, added an intrinsic GaN spacer, and then deposited a nominally 30-nanometer InGaN shell. The rods had a hexagonal cross-section, with six non-polar sidewalls and distinct edges where neighboring facets meet.

To examine those local differences, the investigators combined scanning transmission electron microscopy (STEM) with low-temperature cathodoluminescence (CL). STEM imaging provided structural and compositional contrast, while CL mapped light emission at nanometer-scale locations. Together, the methods connected features in the material to their local optical response.

Imaging reveals indium-rich triangular nanoprisms

High-angle annular dark-field STEM images showed the core, spacer, and InGaN shell. In this imaging mode, brighter contrast indicated regions with higher indium content. At the six vertices of the nanorod’s hexagonal cross-section, the team observed brighter, triangular regions within the shell.

Structural analysis found that each triangular nanoprism was bounded by three equivalent a-plane nanofacets, each approximately 46 nanometers in length. Together, the facets formed an equilateral triangular base. The sharp interfaces between the brighter regions and surrounding material indicated clearly defined domains rather than a gradual, uniform shell composition.

CL mapping confirmed that these edge regions behaved differently from the InGaN on the sidewalls. The sidewall shell showed a strong emission near 400 nanometers, while the nanoprism regions emitted at longer wavelengths, including around 500 nanometers. This redshift, together with the brighter STEM contrast, indicated greater indium incorporation in the nanoprisms.

Emission maps show a composition gradient

A spectral line scan across an individual nanoprism revealed multiple emission contributions as the measurement moved from the GaN core toward the nanorod surface. The observed InGaN peaks were approximately 417, 452, and 500 nanometers. This progression indicates increasing indium concentration toward the outer surface of the nanoprism.

The researchers estimated an indium concentration of about 17% near the inner interface of the nanoprism. For comparison, emission from the initial InGaN layers on the non-polar sidewalls corresponded to an estimated concentration of about 13%. The comparison suggests roughly four percentage points more indium in the nanoprism region than in the initial sidewall layer.

The longest-wavelength signal, near 500 nanometers, was relatively weak. The study associated this lower intensity with possible nonradiative recombination near the surface and reduced crystal quality in that region. The measured emission therefore provides evidence of local composition, but its intensity also reflects other material effects.

Sidewall regions are not compositionally uniform

The sidewall shell also contained areas of higher indium content. Near the nanorod edges, STEM images showed wedge-shaped regions with brighter contrast than the InGaN deposited directly on the GaN spacer. Local CL spectra supported this interpretation: the emission shifted from about 401.5 nanometers at the interface to an overall peak near 406.3 nanometers in the higher-indium wedge region.

These observations show that compositional variation is not limited to the triangular nanoprisms. Both the edges and the sidewalls can contain multiple InGaN domains, each with its own optical signature. A single average measurement across a nanorod could therefore obscure important local differences.

Implications for epitaxial process understanding

The study identifies several factors that may influence indium incorporation, including crystal-facet orientation, strain distribution, surface conditions, and atomic-scale structure. The precise growth mechanism behind the distinct domains was not established. The sharp interfaces and complex three-dimensional geometry suggest that explanations based only on elastic strain may not capture the full process.

For semiconductor process development, the practical lesson is to characterize material at the scale where growth differences occur. Where a device depends on consistent emission or composition, measurements that resolve individual facets and interfaces can reveal variations hidden by ensemble averages. Correlating structural imaging with spatially resolved optical data is one way to distinguish changes in composition from other influences on luminescence.

Conclusion

Direct STEM-CL imaging shows that InGaN/GaN nanorods can develop indium-rich triangular nanoprisms at their edges, alongside higher-indium wedges on the sidewalls. The nanoprisms exhibit a composition gradient toward the surface and longer-wavelength emission than the surrounding shell. For researchers and engineers assessing core-shell growth, these findings underscore the need to account for facet-dependent deposition and local material variation when evaluating nanorod composition and optical behavior.