As semiconductor interconnect pitches shrink, resistance-capacitance (RC) delay becomes an increasingly important design and manufacturing concern. Porous low-k dielectrics such as SiCOH can reduce capacitance, but their porous structure is vulnerable during plasma processing. A study of pulsed plasma etching found that pulsing the RF plasma source reduced damage to porous SiCOH sidewalls and produced more anisotropic etched profiles than continuous-wave operation under the tested conditions.
For process engineers and integration teams, the result highlights a potential way to manage a difficult trade-off: etch the dielectric with the profile required for interconnect patterning while limiting changes that can undermine its low-k properties.
Why porous low-k dielectrics are vulnerable
In back-end-of-line (BEOL) interconnects, reducing capacitance helps address RC delay. SiCOH is used as a low-k dielectric, and introducing pores can lower its dielectric constant further. But those pores also leave the material susceptible to plasma-induced damage during etching.
Plasma ions, reactive radicals and ultraviolet or vacuum-ultraviolet (UV/VUV) radiation can break Si-CH3 bonds in SiCOH. The resulting chemical changes make the material more hydrophilic. It can then interact more readily with moisture, increasing its dielectric constant and potentially degrading the RC-delay benefit the low-k film is intended to provide.
Damage at the etched sidewall is particularly significant in copper/low-k structures because the modified layer can contribute to increased capacitance. The challenge is therefore not only to transfer the pattern, but also to preserve the dielectric condition at the newly exposed sidewalls.
How RF pulsing changes the etch environment
Conventional plasma etching commonly uses continuous-wave (CW) power. With source pulsing, RF power is switched on and off at a selected frequency and duty ratio. This changes plasma conditions over time, including electron density, electron temperature and the balance of reactive species. Those changes can influence etch profile, selectivity, polymer formation and radiation exposure.
The study compared CW operation with a pulsed source in a dual-frequency capacitively coupled plasma system. The 60 MHz source power was pulsed, while a 2 MHz bias remained continuous to provide ion bombardment at the substrate. The reported pulsed condition used a 1 kHz frequency and 50% duty ratio. The process used a C4F8/Ar/O2/N2 gas mixture at 30 mTorr.
In this arrangement, source pulsing does not mean the plasma or etching necessarily stops during the source-off interval. The continuous bias and plasma afterglow can sustain activity. That distinction helps explain why the measured etch rate did not simply fall in proportion to the source-on time.
Etch profile and damage results
The researchers first established a CW etch condition that produced an anisotropic SiCOH profile, then compared it with source-pulsed operation. At the selected CW condition, source power was 100 W and substrate bias was -600 V. Applying source pulsing at the same source power and bias produced a more anisotropic profile, which the study associated with increased sidewall passivation.
The pulsed condition had a lower etch rate than the 100 W CW condition. However, the profile comparison also considered a lower-power CW process selected to give a similar etch rate. The pulsed process still showed a more anisotropic profile than that rate-matched CW condition. This indicates that the profile improvement was not explained solely by reducing average source power.
To estimate sidewall damage, the etched samples were dipped in diluted HF and the resulting sidewall thickness loss was measured. The HF treatment removed material modified by plasma exposure, allowing the researchers to compare the damaged layer. Under the reported test conditions, the pulsed process showed a damaged-layer thickness about 40% lower than the CW process. The sidewall-angle change after dipping was also smaller for the pulsed condition, by 3.3 degrees.
FT-IR measurements provided a complementary indication of chemical change. The ratio of the Si-CH3 signal to the Si-O signal was lower after CW etching than after pulsed etching, consistent with greater carbon depletion in the CW-etched material. These measurements support the conclusion that source pulsing reduced damage in the tested porous SiCOH patterns.
Why pulsing may protect the sidewall
The analysis linked the reduced damage to two related effects. First, pulsed operation promoted a more polymerizing plasma environment. X-ray photoelectron spectroscopy found stronger signals associated with fluorocarbon surface polymer on the pulsed-etched samples. Such a surface layer can act as sidewall passivation during etching.
Time-resolved plasma measurements showed that electron density and temperature declined during the source-off part of the cycle, while plasma species remained present. The authors related these conditions to reduced dissociation of the process gas and a lower proportion of free fluorine relative to CFx species. In the study’s interpretation, this balance supported polymer formation and reduced fluorine diffusion into the SiCOH sidewall.
Optical emission measurements also indicated lower UV emission from the pulsed plasma than from CW operation. Because UV/VUV radiation can contribute to Si-CH3 bond breaking, reduced radiation was identified as another possible contributor to lower damage. The study directly measured UV emission; VUV reduction was discussed as a likely related effect, rather than directly established by the reported optical measurements.
Practical implications for BEOL process development
For BEOL integration teams, RF source pulsing is a process-control option to evaluate when porous low-k sidewall integrity is a priority. The reported results suggest that pulse conditions can influence both the etch profile and the surface chemistry, rather than serving only as a means of reducing delivered power.
Process qualification should consider multiple outputs together, including:
- Etch rate and profile anisotropy
- Sidewall damage and post-etch material loss
- Changes in Si-CH3 bonding or carbon content
- Polymer formation and its role in sidewall passivation
- The effects of pulse frequency and duty ratio on plasma behavior
The study also reported an etch-rate reduction with source pulsing. The magnitude and process significance will depend on the application and integration requirements; the reported experimental result should not be treated as a universal process recipe. The tested gas mixture, reactor configuration, power conditions and material stack are important context for interpreting the findings.
Conclusion
In the investigated dual-frequency CCP process, RF source-pulsed etching produced more anisotropic porous SiCOH profiles and less measured sidewall damage than CW etching. The evidence points to increased fluorocarbon passivation and reduced UV emission as contributing mechanisms, alongside changes in plasma species during the pulse cycle. For manufacturers developing advanced BEOL interconnects, pulsed plasma etching merits evaluation as a way to balance profile control with protection of vulnerable low-k dielectrics, while accounting for its etch-rate trade-off and validating performance within the specific process integration.