SEI growth modeling can help battery developers and technical teams understand one of the processes behind lithium-ion capacity fade. The solid-electrolyte interphase (SEI) forms on a negative electrode when its potential falls outside the electrolyte’s stability window. This passivating layer is necessary for stable operation, but continued growth consumes lithium inventory and can increase resistance to ion and electron transport.

A model of SEI growth on carbon black offers a more detailed explanation of how the process changes during a charge-discharge cycle. Its central idea is that the early SEI is not simply an electronic insulator: it behaves as a mixed ion-electron conductor whose electron conductivity depends on lithium-ion concentration. This helps account for observed differences in growth with voltage, current, and current direction.

Why SEI growth matters for battery performance

SEI formation is one of several coupled processes that influence battery degradation. As the layer grows, it draws lithium from the cell’s available inventory. It can also add a transport barrier, increasing overpotential during operation. Under high-current conditions, added resistance can contribute to resistive heating; increased overpotential for lithium transport can also be associated with lithium plating.

Predicting this evolution is challenging because several mechanisms may affect the growth rate: electron or lithium-ion transport through the SEI, solvent diffusion, reactions at interfaces, and changes in the layer’s composition or structure. Different mechanisms may dominate at different stages. A model that reproduces long-term, square-root-of-time capacity fade is not, by itself, proof that it has identified the correct rate-limiting process.

SEI growth modeling: linking ion concentration and electron transport

The model focuses on the post-first-cycle period, rather than the distinct process of initial SEI formation. It represents a uniform SEI layer on carbon black and couples SEI-forming electrolyte reduction to reversible lithium intercalation in the carbon. The reactions are described using Butler-Volmer kinetics, while current through the SEI and changes in species concentrations affect the reaction rates.

In this framework, lithium ions enter the SEI from the electrolyte. The model assumes local electroneutrality, which links the concentrations of mobile lithium ions and electrons. It then relates electronic conductivity to lithium-ion concentration using a power law. A quadratic relationship is used to represent a non-ideal mixed conductor, consistent with electron hopping through connected, percolating pathways.

The proposed mechanism is that added lithium ions make it easier for electrons to move through the early SEI. Those electrons can reach the outer SEI/electrolyte interface, where they support electrolyte reduction and further layer growth. The conductivity therefore changes with the electrochemical state of the SEI rather than being determined only by its thickness.

Why lithiation and delithiation produce different growth

Experiments on carbon black showed substantially more SEI growth during lithiation than during delithiation, with growth dropping sharply when the current direction reversed. A constant-conductivity model could capture some asymmetry under constant-current operation, partly because the SEI reaction changes how much current remains for intercalation and affects the time spent in each half-cycle. However, that effect alone does not explain asymmetry that persists under potentiostatic conditions.

With concentration-dependent conductivity, current reversal changes the lithium-ion concentration in the SEI. During lithiation, the model predicts increased concentration and improved electronic connectivity, supporting the outer-surface reduction reaction. During delithiation, the concentration falls; the proposed percolating pathways become less connected, reducing electron availability at the reaction interface and suppressing further SEI growth.

This distinction matters for interpreting cycle data. The measured SEI contribution depends not only on how long a battery spends at a given voltage, but also on current magnitude and direction. In the reported carbon-black study, the model reproduced differential-capacity measurements over nominal rates from C/100 to C/5. These results concern early-cycle behavior in the studied system; they do not establish that the same assumptions apply to every electrode material, electrolyte, or operating regime.

What the model means for battery engineering

For battery developers, the practical value of this approach is its attention to transient electrochemical conditions. Treating SEI resistance as a function of thickness alone may miss changes associated with voltage, lithium-ion concentration, current direction, and current magnitude. A degradation model that incorporates these dependencies can provide a more complete framework for analyzing capacity fade during cycling.

The framework also has important limits. It simplifies the electrode as a uniform, one-dimensional layer on a single carbon-black particle, assumes a spatially uniform lithium-ion concentration in the SEI, and uses effective reaction parameters rather than resolving individual SEI-forming chemical reactions. Its conclusions are therefore best understood as a mechanism-based model for the early post-first-cycle regime, not a universal description of SEI evolution over a battery’s full service life.

Conclusion

SEI growth modeling that couples lithium-ion concentration to electron conductivity offers an explanation for the strong dependence of early SEI growth on cycling direction. The model links lithiation to greater electronic connectivity and continued growth, while delithiation reduces electron transport and suppresses the reaction. For engineering teams, the key implication is that cycle history and current direction can matter alongside voltage, time, and layer thickness when interpreting early capacity fade. Applying the framework responsibly requires attention to its material-specific evidence and simplifying assumptions.