Understanding SiC Schottky diode leakage current requires more than choosing a single carrier-transport mechanism. Under reverse bias, carriers can pass over the Schottky barrier through thermionic emission or cross it by tunneling. A combined analysis of these mechanisms offers a clearer way to interpret reverse current–voltage characteristics in 4H-SiC devices, including how their relative contributions change with voltage, temperature and doping concentration.
This distinction matters when engineers assess diode behavior from measured reverse I–V data. A model that considers only one mechanism may not describe the full bias range, particularly around the point where thermionic emission and tunneling contribute currents of similar magnitude.
Why reverse leakage in 4H-SiC needs a combined model
4H-SiC is used in power, high-temperature and high-frequency electronics because of material properties that include a wide band gap, high breakdown fields and high thermal conductivity. In a Schottky barrier diode, however, the reverse current is shaped by the barrier at the metal–semiconductor interface and by the ways carriers can cross it.
At a basic level, thermionic emission describes carriers with enough energy to pass over the potential barrier. Tunneling describes carriers that pass through the barrier, including carriers with lower energy than the barrier maximum. The combined approach treats total current density as the sum of these two contributions:
- Thermionic emission: carrier transport over the Schottky barrier.
- Tunneling: carrier transport through the barrier, represented using a tunneling probability.
The relative share of each process is not fixed across reverse-bias conditions. Separating their contributions therefore helps explain how the measured current changes as the applied voltage and operating temperature vary.
Accounting for image-force barrier lowering
The barrier itself can be modified by the electric field near the metal–semiconductor interface. The model incorporates image-force barrier lowering, which reduces the effective barrier under the conditions considered. This effect is included in the treatment of both thermionic emission and tunneling, rather than being applied to only one current component.
For tunneling, the probability that a carrier crosses the barrier is calculated with the Wentzel–Kramers–Brillouin (WKB) approximation. The barrier profile depends on factors including reverse bias, semiconductor permittivity and donor concentration. Because the barrier profile affects the tunneling probability, changes in bias and doping can influence the tunneling contribution as well as the overall reverse current.
For the thermionic component, the analysis uses a barrier-lowering term in the current expression. Combining these treatments provides a framework for comparing the two components on the same basis and reconstructing their sum against measured reverse characteristics.
Identifying the reverse transition voltage
The reverse transition voltage, often denoted VT, is defined by the intersection of the calculated thermionic-emission and tunneling current components. Below this crossover, thermionic emission is the larger contribution in the reported analysis; above it, tunneling becomes dominant. Near the intersection, the two currents are of comparable magnitude, so neither mechanism alone is an adequate description of the total current.
This crossover is a model-based interpretation of the measured I–V characteristic, not a claim that one process switches off as the other takes over. Both components are included in the total current. Their intersection provides a practical way to identify the bias region where their relative importance changes.
Comparing barrier-height assumptions
The analysis considers two ways to handle the effective Schottky barrier height when extracting its value from reverse I–V data:
- Bias-dependent barrier height: the barrier height is determined for each measured bias point. This approach allows the extracted value to vary with reverse voltage.
- Bias-independent effective barrier height: a single effective value is obtained by averaging values extracted across the measured bias points.
The bias-dependent approach better describes the reported reverse characteristics, particularly at low temperatures and low reverse bias, where the extracted barrier height varies more strongly with bias. The bias-independent approach can show larger differences from measured current at low temperatures. The comparison underscores why barrier-height assumptions should be made explicit when interpreting leakage-current models.
How temperature and doping affect the crossover
For the 4H-SiC diode data analyzed, the experimental reverse transition voltage generally increases with temperature in the high-temperature range and decreases as donor concentration increases. These trends agree with the analytical model used for comparison. The data also show that the bias dependence of the extracted barrier height can be more pronounced at lower temperatures, making the choice of barrier-height model important in that region.
Not every crossover can be established with equal confidence from available measurements. In some cases, reverse I–V data were not available at sufficiently low bias to locate where the two components might intersect. The transition voltage should therefore be interpreted in the context of the measured range and the assumptions used to extract the barrier height.
Practical implications for device analysis
For engineers and technical teams evaluating reverse characteristics, the combined model offers a structured method to:
- separate thermionic and tunneling contributions to total reverse current;
- identify the bias at which their calculated contributions intersect;
- include image-force barrier lowering in both transport mechanisms; and
- compare bias-dependent and bias-independent barrier-height assumptions.
The method was applied to previously published experimental data for 4H-SiC Schottky diodes with different donor concentrations and over a range of temperatures. Its conclusions relate to analysis of those reverse characteristics; the model does not remove the need to consider measurement coverage and the selected assumptions when interpreting a particular device.
Conclusion
Reverse leakage in a 4H-SiC Schottky barrier diode can arise from both carrier emission over the barrier and tunneling through it. Modeling their sum, while accounting for image-force barrier lowering, makes it possible to distinguish the contributions and estimate their crossover voltage. For the cases analyzed, a bias-dependent barrier height provides the more suitable description, especially at low temperature and low reverse bias. For device evaluation, the practical takeaway is to assess both transport mechanisms together and treat the extracted transition voltage in light of the available I–V data.