Vertical GaN diodes are being investigated for power electronics applications where devices must manage high voltage and current. Their performance depends not only on the properties of gallium nitride (GaN), but also on how the device is built. In particular, regrowing semiconductor material to form a p-n junction can introduce an interface where impurities affect current flow. Measurements on nonpolar m-plane GaN diodes show that the type and level of interfacial impurities are associated with important differences in forward and reverse electrical behavior.
Why vertical GaN diodes are of interest
GaN is a wide-bandgap semiconductor considered for power conversion and control, including converters, inverters, motor drives and power supplies. A vertical device conducts through the thickness of the semiconductor rather than primarily along its surface. This geometry is intended to support higher breakdown voltage, low on-resistance and greater current handling, while also offering potential benefits such as reduced current collapse, low parasitic inductance and a compact form factor.
Those advantages depend on the device structure and fabrication. Selective-area doping, for example, can require etching a region and then regrowing material within it. The resulting regrowth interface becomes part of the junction. If the interface contains impurities, it may provide pathways or conditions that affect leakage and conduction. Understanding this interface is therefore important when developing vertical GaN power devices.
Regrowth creates an interface to manage
The reported work examined vertical p-n diodes formed on nonpolar m-plane (10-10) GaN. The devices included a drift region and a p-GaN layer, with the junction either formed during continuous growth or created through a regrowth process. Different regrowth histories were compared, including growth after an interruption, growth after the sample had been stored outside the chamber, and growth following a surface-cleaning treatment.
A further set of structures introduced a thin n-GaN layer before regrowing the p-GaN. In these devices, the inserted n-GaN layer was either 300 or 600 nanometers thick. These variations offered a way to examine how the location and composition of the regrown interface relate to diode behavior.
Electrical characterization included forward and reverse current-voltage measurements, specific on-resistance, reverse blocking behavior and diode ideality factor. Secondary ion mass spectrometry (SIMS) was used to assess impurity profiles, including silicon, carbon and oxygen near the junction. Taken together, the measurements connect processing history and interface composition with device-level electrical characteristics.
What the impurity profiles reveal
The comparisons show that regrowth does not produce a single, uniform electrical outcome. Diodes with moderate interfacial impurity levels exhibited favorable forward and reverse characteristics relative to devices with more problematic impurity combinations. The results therefore point to impurity composition—not simply the presence of a regrowth interface—as an important consideration.
In the reported comparisons, high carbon levels alongside moderate oxygen and silicon levels were also associated with good forward and reverse behavior. By contrast, high oxygen together with high carbon was associated with increased reverse leakage and forward voltage. The highest reverse leakage and forward voltage were observed in samples with high silicon levels and moderate to high oxygen and carbon.
These findings are a reminder that impurity species can have different implications depending on their combination and concentration. A process assessment based only on whether a surface was cleaned, exposed to an interruption or regrown may miss the more relevant question: what impurity profile remains at the electrically active junction?
Implications for device characterization and process development
For engineers and process teams developing regrown GaN structures, the results support evaluating interface chemistry alongside conventional electrical metrics. Forward voltage and on-resistance help describe conduction in the on-state, while reverse leakage and blocking behavior indicate how the device performs under reverse bias. Looking at these measurements together can reveal trade-offs that may not be apparent from a single figure of merit.
- Track the interface: Use impurity profiling such as SIMS to examine species near the metallurgical junction.
- Compare process variants: Distinguish continuous-growth references from regrown structures and document interruptions, storage and surface treatments.
- Assess both bias conditions: Pair forward current-voltage and on-resistance measurements with reverse leakage and blocking measurements.
- Interpret species in combination: Consider the measured levels of carbon, oxygen and silicon together rather than treating each impurity in isolation.
The study focuses on nonpolar m-plane devices and compares them with a continuously grown reference. Its conclusions should be understood in that context; the results do not establish that every regrowth process or GaN device orientation will respond identically.
Conclusion
Regrowth is a route to forming junctions and selectively doped regions in vertical GaN power devices, but the interface it leaves behind can influence electrical performance. In the examined m-plane diodes, impurity combinations were associated with differences in reverse leakage and forward voltage, while moderate impurity levels were compatible with favorable behavior. For device designers and manufacturing teams, the practical lesson is to treat interface control and impurity characterization as part of electrical optimization—not as separate materials checks. Linking process history, SIMS profiles and measurements in both forward and reverse bias provides a more complete basis for refining regrown vertical GaN structures.