Access Official Technical PDF

Share Summary:LinkedInEmail

In miniature electronics manufacturing, too much or too little conductive glue beneath a silicon die can create defects. Excess glue may contribute to internal short circuits, while an insufficient deposit can result in weak bonding. A 3D laser scan inspection system combined with deep learning offers a way to estimate glue volume from PCB surface geometry, both before and after die attachment.

The approach is designed for printed circuit boards (PCBs) built on liquid crystal polymer (LCP) substrates. Rather than relying solely on visual checks by an operator, it captures three-dimensional measurements and uses a neural network to estimate the amount of glue in each region. This is especially relevant after attachment, when the die covers most of the deposit and only a small amount of glue may remain visible around its edges.

Why glue volume is a critical inspection variable

The manufacturing sequence has two main stages: conductive glue is dispensed onto the substrate, then a die or other wire-bondable component is attached. Dispenser pressure is used to control the amount deposited, but the key quality variable is the resulting glue volume.

Operators traditionally inspect the deposit before attachment and the visible glue fillet—the material extending around the die border—afterward. Manual assessment can be time-consuming and subject to human variability. These limitations are particularly challenging in preproduction runs, when process settings may still need adjustment and defect rates can be higher.

Automating this inspection can give production teams a more consistent way to identify potential under- or over-dispensing. It also creates the possibility of checking the attachment after the die is in place, rather than limiting assessment to the exposed glue before assembly.

How 3D laser scan inspection estimates glue volume

The system combines a laser scanning sensor with a modular motion-control setup. The sensor captures measurements from selected PCB regions as three-dimensional point clouds: collections of points representing the scanned surface. A motion controller moves the scanning stages and triggers data acquisition at defined positions.

To reduce scan time, the system uses distance-spaced hardware trigger pulses as the stages move. The scan follows a zig-zag path across each region, rather than taking individual measurements after stopping at every position. The paper reports that this strategy reduced scanning time compared with single measurements at each step, while retaining the measurements needed for the analysis.

For volume estimation, the point cloud is converted into a three-dimensional voxel grid. Each voxel records whether the scanned space contains a surface point. A 3D convolutional neural network, called Regression-Net (RNet), processes this representation and outputs an estimated glue volume.

Training with volume-labelled scans

Training the model requires examples paired with estimated glue volumes. For regions without attached dies, the researchers identified the substrate plane, separated the glue points from the scan, and reconstructed a surface mesh. They then approximated deposit volume from the mesh and its relationship to the substrate plane. These estimates were used to label the point-cloud samples.

Measurements from uncovered glue regions were also used to extend volume labels to corresponding regions after die attachment. This step is important but introduces uncertainty: after attachment, most of the glue is hidden, and the estimated label cannot be treated as a direct scan of the full deposit. Sensor noise, variation in dispensing, and the volume approximation also affect the labels.

Because the initial set of labelled scans was limited, the dataset was augmented. The process included rescanning boards, shifting the region used to crop each point cloud, and adding noise to approximate measurement variation. This helped the models account for differences in scan positioning and data capture.

Estimating volume after die attachment

Inspection after attachment is the more demanding case. The die occludes much of the glue, leaving the system to infer the original volume from visible material around the die and from the measured geometry of the assembled region. RNet was trained separately for different glue-region types and for scans taken before or after attachment.

In the reported evaluation, RNet generally estimated volume more accurately than the alternative 3D architectures tested. Its predictions followed the overall changes in glue quantity across test samples, including when dies were attached. Accuracy was lower in the occluded condition, as expected, and the authors noted larger deviations for some region types where less glue was visible.

The system was also evaluated with two scanning steps, 20 and 50 micrometres. The larger step produced sparser scans and reduced total scanning and prediction time in the reported setup, without substantially changing volume-estimation error in the comparison. This suggests a practical trade-off for production teams: scan density can be selected with inspection time and required accuracy in mind.

What manufacturers should consider

The results demonstrate a method for applying deep learning to 3D inspection data for a specific microelectronics attachment task. They do not eliminate the need to establish appropriate limits for acceptable glue quantities. In the reported work, estimated volumes were used with thresholds informed by expert knowledge to classify potential faults.

For an industrial implementation, several points matter:

  • Inspection timing: Scanning before attachment provides a clearer view of the deposit; scanning afterward can support later-stage checks but relies on partial visibility.
  • Data quality: Point-cloud capture, substrate-plane estimation, and representative training samples all influence the volume estimate.
  • Process coverage: The evaluated setup used multiple glue-region types and simulated a range of deposited quantities. Different products or geometries would require their own assessment.
  • Cycle-time fit: Scan resolution affects acquisition time, so it should be considered alongside the manufacturing process and the inspection decision required.

Conclusion

Combining laser-generated point clouds with a 3D convolutional neural network provides a route to automated PCB glue-volume inspection. The approach can estimate deposits before die placement and, with reduced accuracy, after attachment when most of the glue is obscured. For manufacturers, the practical value lies in making a traditionally manual geometric check more repeatable and in extending inspection to a later stage of assembly. Any deployment should validate scanning settings, volume thresholds, and model performance against the specific PCB regions and process conditions being monitored.

Access Official Technical PDF

About The Author