Access Official Technical PDF

Share Summary:LinkedInEmail

Atomic layer deposition (ALD) gives manufacturers and materials engineers a way to build thin films with precise control over thickness and coverage. Its companion process, molecular layer deposition (MLD), extends this approach to organic and organic–inorganic materials. Together, these techniques can create nanostructured materials for applications ranging from engineered surfaces to catalysts and batteries.

For industrial automation professionals, the significance is not simply that these processes work at the nanoscale. Their surface-controlled growth can coat complex geometries and support repeatable control of material composition. Understanding how the processes work—and where they are being applied—helps teams assess their potential in advanced manufacturing and materials development.

How atomic and molecular layer deposition work

ALD builds an inorganic film through repeated exposures to different gaseous precursors. Each exposure triggers a self-limiting reaction at the surface. Purging between exposures removes excess precursor and gaseous reaction products before the next reactant is introduced. Repeating the cycle adds material in a controlled, layer-by-layer manner.

A common example uses trimethylaluminum and water to deposit aluminum oxide. The first precursor reacts with available surface groups; after purging, water reacts with the modified surface. The sequence can then be repeated. Because growth depends on surface reactions rather than a continuous supply of material to the surface, ALD can produce uniform films and coat high-aspect-ratio structures conformally.

MLD follows a similar alternating, surface-reaction approach but uses molecular building blocks to form organic films or organic–inorganic hybrids. In an alucone process, for example, trimethylaluminum is paired with ethylene glycol. The larger molecular components can produce faster film growth than the corresponding inorganic ALD process, although the deposited material has a different composition and structure.

Building nanostructures across multiple dimensions

Deposition can be combined with templates, particles and other substrate structures to create materials with different shapes. These are commonly grouped by dimensionality: zero-dimensional particles, one-dimensional wires or tubes, two-dimensional films and laminates, and three-dimensional networks or porous structures.

  • Particles and core–shell structures: ALD or MLD coatings can form controlled shells around nanoparticles. In some processes, a coated template is later removed to leave hollow spheres.
  • Nanotubes and nanowires: Deposition inside carbon nanotubes or porous templates can create coated structures or free-standing tubes after the template is removed.
  • Nanolaminates: Alternating films, such as aluminum oxide and titanium dioxide, allow layer thickness and composition to be adjusted to tune material properties.
  • Three-dimensional networks: Conformal deposition on complex templates can preserve intricate internal geometries, including interconnected and porous structures.

These examples show why process control matters: the resulting material depends not only on the selected precursors, but also on the substrate, deposition temperature, cycle sequence and any subsequent treatment. Heating, oxidation or template removal can change a deposited structure into a different material or morphology.

Applications in surface engineering and catalysis

In surface engineering, thin ALD or MLD coatings can modify the chemical, optical, wetting or mechanical behavior of a surface. For example, coatings have been studied to adjust wettability, reinforce nanoparticle films and create multilayer structures with selected optical properties. Because coating thickness and composition can be varied through the deposition sequence, these methods offer a route to tailoring interfaces rather than changing an entire component’s bulk material.

Catalysis is another area where nanoscale control is valuable. ALD has been used to place metal atoms or small clusters on supporting materials and to prepare bimetallic particles. It has also been investigated as a way to apply thin protective coatings around catalyst particles. Such coatings can help limit particle sintering—the loss of dispersion as particles grow or aggregate during heating—while still allowing reactants to reach active surfaces when the coating is appropriately porous.

MLD-derived hybrid coatings have also been explored for catalyst stabilization and photocatalytic materials. In these cases, the composition and post-deposition treatment influence the final structure and activity. The broader engineering lesson is that a coating’s function depends on more than its nominal chemistry: thickness, porosity, interfaces and thermal history all matter.

Implications for batteries and energy storage

In rechargeable batteries, electrode–electrolyte interfaces are important to cycling behavior and material stability. ALD coatings have been investigated as protective layers on electrode materials, while MLD coatings have been studied for modifying silicon and lithium surfaces. These approaches aim to manage interfacial reactions and accommodate changes that occur as electrodes charge and discharge.

Deposition methods can also contribute to the design of nanostructured electrodes and solid-state battery components. ALD and MLD offer control over thin-film thickness and can coat complex structures, characteristics that are useful when designing layered cells or modifying porous electrode materials. Research has also combined the two methods to create thin-film electrode and electrolyte systems. These examples represent specific studies, not a guarantee that any coating will improve performance in every battery chemistry or operating condition.

Practical considerations for process adoption

ALD and MLD are not interchangeable with every vapor-deposition process. Their self-limiting reactions provide a distinct route to controlling film growth, but successful deposition depends on compatible precursor chemistry, suitable process conditions and access to the surfaces being coated. The cost and availability of precursors are also relevant considerations; the review notes that precursor supply and demand affect process costs.

For engineering teams, evaluation should begin with the intended function of the coating and the geometry of the substrate. Questions include whether the film must be inorganic or hybrid, whether conformal coverage is essential, what thermal conditions the substrate can tolerate, and whether post-processing is required. These factors help determine whether ALD, MLD or a combined sequence is appropriate.

Conclusion

Atomic layer deposition and molecular layer deposition provide precise ways to build and modify nanostructured materials, from particle coatings to multilayer films and three-dimensional networks. Their controlled growth and conformal coverage have supported work in surface engineering, catalysis and batteries. For industrial decision-makers, the practical opportunity lies in matching those capabilities to a specific materials challenge—and accounting for precursor chemistry, substrate geometry, temperature and post-treatment before moving toward process implementation.

Access Official Technical PDF

About The Author