Access Official Technical PDF

Share Summary:LinkedInEmail

For manufacturers handling sensitive semiconductor components, an ESD current threshold can provide a more practical view of risk than a withstand-voltage rating alone. Human Body Model (HBM) data are widely available, but they describe performance under a particular test waveform. Discharges from charged conductors, insulators, equipment, or materials can have different current profiles and durations. Understanding how current and pulse duration contribute to device damage helps engineers evaluate ESD sources and protection measures in an electronics assembly environment.

Why HBM withstand voltage does not tell the whole story

An HBM rating identifies the largest test-source voltage a device withstands under the defined HBM test conditions. It is useful for comparing or specifying component susceptibility, but it is not a direct measure of how the device will respond to every real-world discharge. In particular, the rating alone does not establish the risk from charged conductors or insulating materials whose discharge waveforms differ from the HBM pulse.

For energy-sensitive devices, damage is commonly associated with energy dissipated in a small internal region as discharge current flows. In a semiconductor junction, for example, intense local heating can cause failure. The current is therefore an important parameter when assessing the potential threat from an ESD source. A material or item can be evaluated by considering the maximum current it may deliver during a discharge, while also accounting for pulse duration and waveform.

How device damage relates to pulse duration

A simplified model represents the affected part of a device as an effective resistance and a junction voltage. Current through these elements produces heat in the damage region. Failure can occur when the region’s temperature rises beyond a critical level, such as a material’s melting point. The required heating depends on the region’s size and material properties, as well as how quickly heat can move into surrounding areas.

For very short pulses, heat has little time to escape. The pulse must deliver enough energy to raise the damage region to its failure temperature. At intermediate durations, some heat diffuses away, so more total energy may be needed. For sufficiently long pulses, heat loss to surrounding material becomes significant and the required failure power approaches a steady level. Consequently, the power needed for failure generally falls as pulse duration increases, until that steady condition is reached.

This thermal behavior leads to different current-versus-duration relationships. For junction-related failure, where the junction voltage is the dominant part of the dissipated power, the estimated failure current decreases approximately with pulse duration to the power of -0.5. For metallization burnout, where resistive heating dominates, the relationship is less steep, approximating a duration exponent of -0.25. The exact failure mechanism may not be known for a given component, so the more conservative applicable current limit should be used.

Estimating an ESD current threshold from HBM data

HBM test data can provide a reference point for estimating a device’s peak current threshold. In the HBM circuit, a 1,500-ohm series resistance largely determines the current when the voltage across the device is small. The HBM withstand voltage can therefore be used to estimate the corresponding peak current at the test pulse duration, approximately 150 nanoseconds.

That reference current can then be adjusted for other pulse durations using the duration relationships described above. The resulting current-duration curves define an estimated boundary: pulses below the conservative threshold are treated as being within an ESD safe area, while pulses above it may present a damage risk. This is an analytical estimate, not a replacement for appropriate component qualification or evaluation of the actual ESD source.

For practical use, the method offers a way to connect routinely available device HBM data with laboratory assessment of ESD threats from equipment and materials. It also shifts attention from voltage alone to the peak current and duration that a source can produce.

Waveform shape changes the assessment

Real ESD pulses do not all have the same shape. Many discharges, including those from charged insulating materials, decay exponentially. Discharges from charged conductive objects may also be unidirectional exponential pulses or oscillatory pulses with an exponentially decaying envelope. An oscillatory discharge generally dissipates less energy in the device than a unidirectional discharge with the same peak amplitude and duration because its current repeatedly returns toward zero. Treating it like a unidirectional exponential pulse provides a conservative approach in the cases described.

A rectangular transmission-line pulse (TLP) is a more demanding waveform for this comparison: it maintains peak current throughout its duration. For a TLP with duration set equal to the time constant of a comparable RC pulse, the estimated current threshold depends on the dominant failure mechanism:

  • When resistive heating dominates, the TLP threshold is estimated at about 0.71 times the comparable RC threshold.
  • When junction-voltage-related dissipation dominates, the thresholds are estimated to be equal.

Using 0.71 of the RC threshold provides a margin for the more severe resistive-heating case. Unusual waveforms may need individual assessment rather than being assumed equivalent to a standard exponential or rectangular pulse.

Applying the method in an ESD control program

For engineers, system integrators, and plant teams, the method supports a structured comparison between an ESD source and the susceptibility of the devices being handled. A practical assessment can:

  • Identify whether the component’s likely failure mechanism is energy-related.
  • Use available HBM data to establish a reference peak current.
  • Account for the duration and shape of the expected discharge.
  • Compare the estimated source current with the conservative current-duration boundary.

The result can inform laboratory evaluation of ESD control materials and equipment used in an ESD Protected Area. It does not imply that HBM voltage ratings alone capture every hazard, nor does a theoretical boundary remove the need to understand the source waveform.

Conclusion

ESD risk to energy-sensitive semiconductor devices depends on more than source voltage. Internal heating, peak discharge current, pulse duration, and waveform shape all influence whether a damaging temperature can be reached. HBM data offer a useful starting point for estimating an ESD current threshold across a range of durations, while conservative derating and waveform comparisons help extend that estimate beyond the standard test pulse. For industrial electronics handling, this approach provides a clearer basis for evaluating ESD sources and selecting protection measures without treating a single withstand-voltage figure as a universal measure of risk.

Access Official Technical PDF

About The Author