Reactive material jetting of polyimide offers a way to insulate selected points in a printed circuit rather than separating entire conductive layers with a dielectric board. In a demonstrated approach, a polyimide precursor is deposited between crossing silver tracks and converted to a solid insulating film through heating. The result is a circuit architecture that can reproduce some functions of a double-sided PCB while keeping the printed tracks on one side of the substrate.
For electronics manufacturers and system designers, the key idea is selective deposition: put dielectric material where electrical isolation is needed, and avoid adding it where it is not. This could give additive manufacturing processes more freedom to produce compact or bespoke circuit layouts, particularly for lower-volume applications. The approach also depends on careful control of ink behavior, curing and the geometry of each insulating patch.
Why selective insulation matters in printed circuits
In a single-sided circuit, conductive tracks cannot cross without risking an electrical short. Conventional double-sided boards address this constraint by routing conductors on separate sides of a board, with insulation between them. Another strategy is to place a small insulating bridge at a crossover so that one track can pass over another.
Material jetting (MJ) is suited to this localized approach because it deposits small droplets only at specified locations. Multiple drop-on-demand printheads can be used to place different functional inks, such as conductive silver and a polymer precursor, in sequence. Instead of applying a dielectric layer across the whole circuit, the process can build a small insulating feature at each required intersection.
This design principle may simplify the fabrication of customized circuits and reduce the need to assemble separately printed board layers. It does not eliminate the need for design and process validation: the insulating patch must fully separate the conductors, and the conductive ink must form a continuous track over the patch.
How reactive material jetting forms polyimide
Polyimides are used as dielectric and protective materials in electronic applications, in part because of their thermal stability and electrical properties. However, the finished polymer is not necessarily the easiest material to jet directly. The demonstrated process instead prints a polyamic acid (PAA) precursor ink and converts it into polyimide through thermal imidisation.
As a deposited droplet heats, its solvents evaporate while the precursor undergoes a chemical transformation. During imidisation, water is released and new bonds form as PAA becomes polyimide. These physical and chemical changes take place together, so substrate temperature affects both how far the droplet spreads and how the film solidifies.
The reported ink contained 20 wt% PAA and was jetted using a 10-picolitre cartridge. It was deposited onto heated glass substrates at temperatures of 120°C, 150°C and 180°C. At 180°C, followed by 15 minutes of additional heating, the printed precursor was almost fully imidised. This shows why process planning must account for both deposition and post-deposition heating, rather than treating printing as the only stage that defines the material.
Film quality depends on temperature and feature size
Substrate temperature influenced the shape of individual droplets and the surface of printed films. At higher temperatures, faster solvent evaporation left less time for droplets to spread. The resulting solidified droplets had smaller diameters and greater thickness. Higher temperatures also improved film surface quality in the reported tests, with lower roughness for single-layer films and more clearly defined edges.
Ink formulation also mattered. The updated PAA ink showed no obvious coffee-ring effect in the reported observations. Such drying patterns can concentrate material at a droplet’s perimeter and create uneven films, which is undesirable when a dielectric feature must provide reliable separation. The study attributed the improved behavior to the formulation’s relatively high PAA concentration and dual-solvent system.
Patch dimensions presented another design trade-off. Insulating squares from 200 by 200 micrometres to 500 by 500 micrometres were printed between crossing silver tracks. Smaller patches could form a pronounced bump with a steep edge. Silver ink deposited over that edge tended to flow down the slope and collect at the patch boundary, reducing the continuity of the upper track. Larger patches reduced this issue in the tested structures.
For engineers developing similar processes, this finding highlights the connection between dielectric geometry and conductor quality. A crossover design cannot be assessed solely by its electrical isolation; the printed topography must also support a continuous conductive path.
Electrical and thermal properties demonstrated
The printed polyimide film had a measured relative permittivity of 3.41 ± 0.09 at 1 kHz, comparable to the commercial polyimide film cited in the study. Thermogravimetric analysis indicated good thermal stability for films that had been printed and post-treated at 180°C for 15 minutes, with no obvious weight loss below 400°C under the reported test conditions. The paper also reports a degradation temperature around 500°C for the printed material.
These measurements characterize the material in the study; they should not be treated as a complete qualification for a production circuit. Application-specific evaluation would still need to consider the full stack-up, operating environment, conductor behavior and the repeatability of the printing and heating process.
Practical implications for circuit design
The demonstration used two crossing silver tracks with a 500-by-500-micrometre polyimide patch at the crossover. The printed circuit operated an LED without a short circuit. This establishes the feasibility of the localized-insulator concept, while leaving broader production questions to be addressed for each use case.
When assessing reactive material jetting for electronic assemblies, teams should consider:
- Track routing: Identify where crossings are necessary and place dielectric patches only at those locations.
- Patch topography: Select dimensions that provide adequate separation while avoiding steep edges that disrupt the overlying conductor.
- Thermal process: Account for solvent evaporation and imidisation, including any required post-heating.
- Film consistency: Inspect surface roughness, edges and potential defects across single- and multilayer features.
- Electrical validation: Verify isolation at crossovers and continuity of tracks in the intended circuit design.
Conclusion
Reactive material jetting of a polyimide precursor can create localized dielectric bridges between intersecting conductive tracks, providing an alternative to separating entire circuit layers. The approach combines selective deposition with thermal conversion, but its success depends on balancing cure conditions, film uniformity and patch geometry. For engineers exploring additive manufacturing electronics, it presents a practical design option for compact, customized circuits—one that requires careful process development and validation for the intended application.