Access Official Technical PDF

Share Summary:LinkedInEmail

As extreme ultraviolet (EUV) lithography moves into advanced semiconductor manufacturing, the resist and development steps remain critical to pattern fidelity. Dry EUV lithography offers a different approach to these steps: apply the resist from a vapor-phase process, then use a dry etch to develop the exposed pattern. Results reported for this process platform indicate that removing liquid developer may help preserve fine features that can collapse during conventional solvent-based development.

The approach is relevant to process engineers and manufacturing teams evaluating how resist materials, patterning methods, and integration choices affect yield and process control. It is not simply a change in developer chemistry; it combines a distinct film deposition method with a different way to remove unexposed material.

How the dry EUV lithography process works

The resist film is formed using reactive organometallic precursors in a vapor-phase deposition process. The resulting films were described as uniform and homogeneous, and stable in air and visible light. Unlike typical spin-on resist processes, the deposited film thickness was reported to be relatively insensitive to substrate surface chemistry. Film thickness can therefore be controlled through deposition time, according to the reported work.

After EUV exposure, a bake step induces crosslinking and densification in exposed regions. The unexposed areas remain hydrophobic and soluble in common organic solvents. Initial lithographic characterization used conventional negative-tone development, in which solvent removes the unexposed material. The process was also evaluated with a dry etch development step selective for unexposed film.

This distinction matters: the resist deposition is dry in both comparisons, but only the newer development route avoids liquid developer. Combining vapor deposition with dry etch development creates the fully dry patterning process described in the workshop abstract.

Patterning results and process-window implications

Tests on NXE-3400 EUV systems at IMEC and ASML reported a dose to size of approximately 45 mJ/cm² for 16 nm half-pitch lines in 32 nm-pitch dense line-and-space patterns. That dose showed little sensitivity to film thickness across the tested 10–25 nm range.

For a 20 nm baseline film, the reported process resolved 13 nm half-pitch line-and-space patterns at 48 mJ/cm², with line-width roughness (LWR) of 2.7 nm and a Z-factor of 0.77. At 16 nm half-pitch, full-wafer critical-dimension uniformity was reported at 3σ of 2.4%. In-lot dose-to-size stability and variability were below 1 mJ/cm² at 3σ.

The more significant reported difference emerged when comparing dry etch development with solvent development. Full-wafer focus-exposure matrix comparisons of otherwise identical dry-deposited films showed a larger pattern-collapse-free process window with dry development. In one example, dense underexposed features with critical dimensions well below the 13 nm target—around 10 nm—remained standing after dry development. Corresponding features following solvent development were absent because of delamination or collapse.

Why avoiding liquid development may help

During solvent development, liquid between tightly spaced features must evaporate. The associated capillary forces can act on small, fragile patterns. As dimensions shrink, those forces can contribute to feature deformation, collapse, or delamination. Dry etch development avoids solvent evaporation from between the features, which provides a plausible process-level explanation for the improved collapse-free window reported in the comparison.

The abstract also reports reduced LWR and Z-factor with dry development, along with potential cost and environmental advantages associated with eliminating liquid developers. These are process-platform findings, not a guarantee that every layer or device design will see the same benefit. Integration requirements and patterning conditions still need to be evaluated for the intended application.

What manufacturing teams should evaluate

For engineers assessing this approach, the results point to several practical considerations:

  • Film control: Vapor deposition links thickness to deposition time and was reported to be less sensitive to substrate surface chemistry than spin-on application.
  • Pattern integrity: The dry development comparison highlights feature survival, particularly for underexposed patterns that may be vulnerable to collapse.
  • Process metrics: Dose-to-size, LWR, Z-factor, wafer CD uniformity, and in-lot stability provide useful dimensions for assessing lithographic performance.
  • Integration: A dry resist and development sequence changes the materials and process steps that must be considered alongside exposure and bake.

The reported platform was described as applicable to high-volume EUV manufacturing, but the workshop results should be understood as process-development evidence rather than proof of universal production readiness. The process was also extended in exposure demonstrations to 9 nm half-pitch using the 0.5 NA MET5 micro-field exposure tool at Lawrence Berkeley National Laboratory.

Implications for advanced EUV patterning

As semiconductor features continue to shrink, lithography performance depends on more than optical resolution. Resist behavior and the steps used to form and develop patterns influence whether fine features remain intact across a usable process window. A dry EUV process addresses part of this challenge by pairing vapor-phase film formation with selective dry removal of unexposed resist.

For manufacturing and integration teams, the key takeaway is to evaluate the complete patterning sequence—not just the exposure dose or resist film. The reported results suggest that eliminating liquid development can improve pattern stability in demanding conditions, while offering a route to lower LWR and a wider collapse-free window. Further assessment should focus on how these benefits translate to specific layers, layouts, and production requirements.

Access Official Technical PDF

About The Author