Solid-state hydrogen storage is being explored as an alternative to storing hydrogen as a compressed gas or cryogenic liquid. One experimental approach uses a proton battery with a porous activated-carbon electrode: electrical energy splits water, and hydrogen is stored in ionic form in the carbon during charging. Testing two catalyst loadings shows how electrode and catalyst choices can influence the charging and discharging process.

How hydrogen storage works in a proton battery

The tested cell operated in two modes. In electrolyser mode, or charging, an applied electrical potential drives water dissociation. Oxygen is released, while hydrogen ions move through the membrane and toward the activated-carbon storage electrode. The study describes hydrogen retention as electrochemical adsorption, involving hydrogen associated with the carbon’s pores and internal surfaces.

During fuel-cell mode, or discharging, the stored hydrogen is released. Hydrogen is split into protons and electrons; protons return through the polymer electrolyte membrane, while electrons travel through an external circuit and provide electrical output. Oxygen supplied to the cell reacts with the protons and electrons to reform water.

This configuration integrates hydrogen generation, storage and subsequent use in one cell. It differs from systems that generate hydrogen for storage in a separate vessel. The reported experiment evaluated a single cell and does not establish commercial-scale performance.

Why use activated carbon from Prosopis juliflora?

The researchers made activated carbon from Prosopis juliflora wood, a locally available shrub in India. The wood was converted to charcoal in a controlled oven at 400°C, crushed and sieved. The selected carbon particles, designated aC-106, were chemically activated using potassium hydroxide. The resulting powder was mixed with a polytetrafluoroethylene binder and pressed into a self-standing porous electrode.

Particle size affected electrode fabrication. The researchers selected the 106-micron material because coarser particles required more pressure and time to form an electrode and could produce brittle electrodes. Finer particles needed more binder, which risked covering carbon pores. Preserving accessible pores matters because they provide sites where hydrogen can be retained.

Surface-area measurements also indicated a change after activation. The reported BET surface area increased from 161.219 m²/g for the carbon to 205.886 m²/g for the activated carbon. The measured pore diameter was 3.698 nm before activation and 3.337 nm afterward. These material properties help characterize the electrode, but surface area alone does not establish the hydrogen capacity of a complete battery.

Catalyst loading and charging behavior

The comparison used two membrane-electrode assemblies (MEAs), with iridium oxide on the oxygen side and platinum black on the hydrogen side. Each catalyst was loaded at either 1 mg/cm² or 2 mg/cm². The cell had a 2.5 × 2.5 cm² active area, and the activated-carbon electrode contained 0.8 g of carbon.

Charging involved applying voltage in steps, up to 3.9 V, while recording current. Water dissociation was observed to begin at a cut-in voltage of 1.5 V. Both MEAs were charged for 3.16 hours, but the higher-loading MEA drew more current: 370 mA compared with 270 mA for the lower-loading assembly. The reported hydrogen gas volumes were 5 cm³ and 4.5 cm³, respectively.

The higher catalyst loading was associated with earlier and stronger water dissociation and hydrogen generation. However, the process also has a practical endpoint: once the carbon electrode approaches saturation, additional hydrogen ions are more likely to combine into hydrogen gas rather than remain stored in the electrode. The study therefore highlights a trade-off between accelerating reactions and directing hydrogen toward storage rather than gas production.

What the discharge results show

During discharge, the higher-loading MEA produced a reported current of 55 mA, compared with 45 mA for the lower-loading MEA. The authors also reported that the higher-loading configuration maintained a higher voltage and met the applied load for longer in their test. These observations are specific to the experimental cell and conditions; they should not be treated as a general performance guarantee for other proton-battery designs.

Reported storage values depend on which measurement is being considered. The study’s discharge calculations give hydrogen released from the activated carbon equivalent to 0.41 wt.% for the 1 mg/cm² MEA and 0.51 wt.% for the 2 mg/cm² MEA. These discharge figures are distinct from the larger hydrogen-generation and storage estimates calculated during charging. For system evaluation, it is important to distinguish hydrogen produced, hydrogen retained in the electrode and hydrogen recovered during discharge.

Practical implications for development

For engineers and technical decision-makers, the experiment illustrates several design considerations:

  • Electrode porosity and fabrication: Particle size and binder content influence whether a porous, mechanically usable electrode can be made.
  • Catalyst loading: Increasing loading affected reaction rates and discharge behavior, but also influenced hydrogen gas formation.
  • Measurement basis: Charging estimates and discharge recovery are not interchangeable measures of storage capacity.
  • System integration: The cell combines electrolysis, hydrogen retention and fuel-cell operation, so each operating mode must be assessed.

The authors identify alternative catalysts and proton-conducting media, including protic ionic liquids and proton-conducting gels, as areas for further investigation. Those possibilities remain future work rather than demonstrated improvements in this experiment.

Conclusion

The study demonstrates the experimental feasibility of storing hydrogen electrochemically in an activated-carbon electrode within a proton battery. In the tested cell, increasing catalyst loading from 1 mg/cm² to 2 mg/cm² was associated with stronger charging activity and higher reported discharge values, while also affecting hydrogen generation. The practical lesson is to evaluate catalyst loading alongside electrode structure and recovered hydrogen—not generation figures alone—when assessing solid-state hydrogen storage concepts for future energy systems.