InP/ZnS quantum dot emission can reveal more than a material’s peak colour and brightness. Its spectral shape and decay over time can also provide clues about defects in the quantum dot structure. In a spectroscopic characterization of InP/ZnS core-shell quantum dots, a broad low-energy emission tail extended beyond the main band-edge peak. Time-resolved measurements showed that this tail had a substantially longer lifetime, supporting an interpretation of emission from trapped charge carriers.

For materials developers and technical teams evaluating optical emitters, the result illustrates why combining steady-state and time-resolved measurements can be valuable. A spectrum identifies where the sample emits; lifetime measurements help distinguish emission processes that overlap in wavelength.

Why the InP/ZnS structure matters

Indium phosphide quantum dots have attracted interest as an alternative to traditional quantum dots containing heavy metals such as cadmium and lead. However, InP dots composed only of a core are non-emissive in the system described here. Non-radiative recombination at surface trap states prevents the core from producing useful photoluminescence.

A higher-bandgap semiconductor shell, such as zinc sulphide, can be grown around the InP core. This core-shell heterostructure helps passivate surface trap states and can greatly increase photoluminescence quantum yield. The shell’s composition and thickness therefore matter: understanding their relationship to optical behaviour can help guide efforts to improve brightness, stability and colour range.

Even with a shell, however, the emission spectrum may contain evidence that passivation is incomplete. Examining such features can help researchers assess how a synthesis process may need to be adjusted.

Reading the steady-state spectrum

The InP/ZnS quantum dots were prepared in toluene at an absorbance of 0.15 at 500 nm. Absorption and photoluminescence were measured using an FS5 spectrofluorometer. The instrument configuration included a cuvette holder, a pulsed 405 nm diode laser, time-correlated single photon counting (TCSPC) electronics and an extended-range PMT-980 detector.

The steady-state photoluminescence spectrum showed a pronounced band-edge peak at 620 nm, with a full width at half maximum (FWHM) of 65 nm. Alongside this main feature was a broad, lower-energy tail extending into the near-infrared. The tail was detectable using the PMT-980, which has sensitivity out to approximately 950 nm. The application note states that this detector provides 80 nm more detection range than the standard PMT-900, making extended detector coverage relevant when a sample emits at longer wavelengths.

The broad tail had been observed previously in InP/ZnS quantum dots and is indicative of trap emission. But a spectral tail alone does not establish how it is produced. To investigate whether it behaved differently from band-edge emission, the measurement also examined photoluminescence decay as a function of emission wavelength.

Time-resolved measurements distinguish emission behaviour

TCSPC was used to build a time-resolved emission spectrum (TRES). The sample was excited with the 405 nm picosecond pulsed diode laser, and decay information was collected across emission wavelengths. The TRES showed that the photoluminescence lifetime increased substantially at longer wavelengths.

For a closer comparison, decays were measured at the 620 nm band-edge peak and at 775 nm in the tail region. The measurements were fitted with four exponential components, and an intensity-weighted average lifetime was calculated. The band-edge emission had an average lifetime of 31.2 ns, while the tail emission lifetime was 348 ns.

This order-of-magnitude difference supports the interpretation that the two spectral regions arise from different processes. In the proposed mechanism, an electron near the conduction-band edge becomes trapped at a surface defect in the InP core. The trapped electron then recombines radiatively with a hole in the valence band, producing longer-wavelength light. The slower decay in the tail region is consistent with this proposed trap-mediated pathway.

What the emission tail may indicate

The findings suggest that the ZnS shell may not fully cover or passivate the InP core. If surface defects remain accessible, they can provide states within the bandgap that contribute to trap emission. The application note therefore identifies deposition of a thicker ZnS shell as a possible direction for adjusting the synthesis procedure.

This is an interpretation of the measured optical behaviour, not proof that shell thickness is the only factor involved. The practical value of the combined measurements is that they provide evidence to inform further investigation: the spectrum identifies the long-wavelength feature, while the lifetime comparison helps connect it to a distinct emission pathway.

Why combine absorption, emission and lifetime data?

Measuring absorption, photoluminescence and lifetime on one instrument can provide a more connected view of a sample’s optical properties. Absorption and steady-state emission help characterize the spectral response, while time-resolved photoluminescence reveals how emission evolves after excitation. In this case, the extended-range detector was important for capturing the near-infrared tail, and TCSPC enabled comparison of decay behaviour at selected wavelengths.

For researchers developing quantum dot emitters, these complementary measurements can help establish structure-property relationships. Rather than relying only on the position and width of the main emission peak, teams can also look for weaker spectral features and compare their lifetimes with those of the principal band-edge emission.

Conclusion

InP/ZnS quantum dot emission included a distinct 620 nm band-edge peak and a broad low-energy tail extending toward the near-infrared. The tail’s 348 ns average lifetime, compared with 31.2 ns at the band-edge peak, supports its attribution to trap-related emission. The measurements suggest that incomplete ZnS passivation may be involved and that shell growth could warrant further optimization. For materials characterization, the broader lesson is practical: combining steady-state spectra with wavelength-resolved lifetime data can expose emission mechanisms that a peak measurement alone may miss.